Abstract


Beige kaolin clays were crushed and sieved. The mineral was characterized by X-ray diffraction and chemically analyzed by atomic absorption spectrophotometry. The material below 37 microns was leached with oxalic acid. A study of main variables of the leaching process in different ranges was realized: time (0 to 120 min), temperature (25 to 100 C) and acid concentration (0.01 to 0.5 M). Crystallographic analysis of the initial sample indicates the presence of kaolinite, iron oxides in the form of magnetite and iron-titanium oxides. By this method it was possible to obtain iron extraction percentages over 80% and whiteness index above to 90%.



Research Product




Related articles

SÍNTESIS Y CARACTERIZACIÓN DE CaMnO3 DOPADA CON LANTANO OBTENIDA MEDIANTE EL MÉTODO DE COMBUSTIÓN

BENEFICIO DE CAOLÍN PROCEDENTE DEL MUNICIPIO DE AGUA BLANCA POR FLOTACIÓN INVERSA: PRUEBAS PRELIMINA...

EXTRACCIÓN LÍQUIDO-LÍQUIDO DE Zn (II) EN DIFERENTES MEDIOS EMPLEANDO COMO EXTRACTANTE EL LÍQUIDO IÓN...

Evaluación del tamaño de partícula de manganitas de calcio dopadas con europio, sintetizadas por el ...

STRUCTURAL IDENTIFICATION AND MAGNETIC BEHAVIOR OF CaMnOOBTENIDE VIA CO-PRECIPITATION

BLEACHING OF BROWN COLORED KAOLINITIC CLAYS BY DISPERSION AND SETTLING

Purificación del caolín por electrólisis

SEPARATION OF Fe OXIDES FROM CAOLIN BY SIMPLE ASPHETATION

DECOLORIZATION OF KAOLINIFEROUS CLAYS BY LEACHING TO OBTAIN KAOLIN WITH A HIGH CONTENT OF...

STUDY OF THE EFFECT OF THE SYNTHESIS TEMPERATURE IN THE PRODUCTION OF CALCIUM MANGANITES DOPED WITH A...